PBAT and PLA/PBAT Film Hydrolysis: A Guide for Blown-Film Converters

Explore the latest trends, technical innovations, and market intelligence in functional materials and global chemical supply chains.

Browse by Category

Need a Custom Quote?

Connect with our team for tailored sourcing solutions.

PBAT and PLA/PBAT Film Hydrolysis: A Guide for Blown-Film Converters

Illustration of tensile testing and heat-seal inspection for PBAT film

Introduction

A blown-film converter may face an unstable bubble during production or bags that tear more easily after warehouse storage. Separate the two problems before adjusting the additive package. Record line behavior and test fresh film before comparing aged rolls.

How the PBAT backbone changes in humid conditions

PBAT contains butylene adipate and butylene terephthalate units. Both provide ester linkages susceptible to hydrolysis. The diagram shows one representative ester at a butylene segment. In a PLA/PBAT blend, both resins can contribute to changes in molecular weight, while blend morphology and filler dispersion can also affect tear and elongation.

Figure 1. PBAT hydrolysis and carbodiimide stabilization

1. Ester-bond cleavage
P–C(=O)–O–(CH₂)₄–O–P + H₂O → P–COOH + HO–(CH₂)₄–O–P

2. Capture of the carboxyl end group
P–COOH + R¹–N=C=N–R² → O-acylisourea intermediate → N-acylurea adduct

P denotes a polymer segment and R denotes an organic residue. These representative reactions show how cleavage creates acid ends and how carbodiimide can consume those ends, reducing their contribution to further hydrolysis.

Test both directions in the finished film

Hold resin ratio, filler loading, gauge, blow-up ratio and conditioning constant across the trial. Record melt pressure and bubble stability during production. Measure tear and tensile elongation in machine and transverse directions, and add seal strength if bag failure occurs at the seam. Retain samples from the same roll for the fresh and aged comparison.

A practical selection guide

Observed problem What to check What to evaluate first
Bubble instability or gauge variation at startup Review feed moisture, line settings and melt rheology. Process correction and, where justified, a KL-180 trial
Rolls pass release testing but lose tear or elongation in storage Compare fresh and aged film at fixed gauge and environmental conditions. HyMax® stabilization
Seal failure dominates returns Measure seal strength and identify the failure location and sealing window. Review the film and sealing process together

How to qualify HyMax® and KL-180

Select a candidate HyMax® grade based on the complete blend, including PLA proportion, carrier compatibility and fillers. Ask Langyi to review the film recipe and route before pairing an anti-hydrolysis agent with KL-180. For certified compostable bags or films, confirm the finished formulation within the applicable certification process.

Run a dried, additive-free control and a HyMax®-only formulation at supplier-recommended levels. Add a KL-180-only trial where a defined melt-processing issue warrants it. Record resin and additive lots, active content or let-down, drying and processing history. Compare both initial and aged results against a predefined acceptance threshold before deciding whether to try a combination.

Frequently asked questions

Can one melt-flow result explain poor film performance?

Use melt flow as a screening indicator. Verify bubble stability, film directionality, gauge and tear or seal performance on the actual line.

Can a hydrolysis stabilizer replace resin drying?

Follow the resin supplier’s drying guidance and record moisture at the feed point. An additive trial is easier to interpret when every formulation starts from a comparable moisture history.

Discuss your application with Langyi